背景:#EDF0F5 #FAFBE6 #FFF2E2 #FDE6E0 #F3FFE1 #DAFAF3 #EAEAEF 默认  
阅读内容

景泰蓝英文导游辞

[日期:2007-09-17] 来源:  作者: [字体: ]

海淀部

国贸部

北三环部

热线:010-51286580
电话:82191315 82191316
传真:010-82191316
MSN:jiayinte2005@hotmail.com
E-mail: jiayinte@163.com
公司地址:西直门长河湾国际公寓B16单元1001室(邻近西直门地铁、城铁B口500米)

热线:010-65812169, 65811168
电话:65815980 ,65815902
传真: 65815902
手机:13910631654
E-mail: LLLL-2008@126.com
jiayinte@263.net
公司地址: 北京市建国路99910

小语种专线:010-64203637
英语专线: 010-64201948
24
小时翻译热线: 13911235215
E-mail: jiayinte@126.com
公司地址:北京市东城区和平里化工部规划院241

 Tel:021-61416565

 MSN: jiayinte2005@hotmail.com  E-mail: jiayinte@163.com

 公司地址上海市人民路885号淮海中华大厦1505

广  Tel:020-22829302

  MSN:jiayinte-2006@hotmail.com   E-mail:jiayinte@126.com

 公司地址:广东省广州市越秀区东风中路350


Copyright © 1998-2007 Beijing GIANT TRANSLATION Co.,Ltd. All rights reserved.
北京佳 音特翻译公司 版权所有 京ICP备06026274号
 

Cloisonne is a famous traditional enamel ware, known as the "Blue of Jingtai" in China, with a history of over 500 years. it was so called "blue" was the typical colour used for enamelling and "Jingtai" was the reign title of the 7th Ming Emperor. Enamel ware became very popular during the Emperor's reign. There is a great variety of products, such as vase, jar, bowl,plate, box and ash-tray. They are brilliant in colours and splendid in design.

  Cloisonne is one of the famous arts and crafts of Beijing.The making of cloisonne requires rather elaborate and complicated processes; base-hammering, copper-strip inlay, soldering, enamel-filling, enamel-firing, polishing and gilding. The products are featured by excellent quality. The skill and workmanship have been handed down from the Ming Dynasty. Quite a number of new varieties have been created. it enjoys a high reputation both at home and abroad. They are mostly for export.

  CLOISONNE-MAKING

  The first step is body making. The material used for making the bodyis copper, because copper is easily hammered and stretched. This step requires a sound judgement in shaping and uniformity of thickness and weight. It is in fact the work of the copper smith. The only difference is that when an article is well shaped, the copper smith‘s  work  is  finished,  whereas the cloisonne craftsman’s work is just on the the start.

  The second step is filigree soldering. This step requires great care and high creativeness. The artisan adheres copper strips onto the body. These strips are of 1/16 inch in diameter and of lengths as the artisan desires. The strips or filigree thus adhered make up a complicated but complete pattern. The artisan has a blueprint in mind and he can make full use of his experience, imagination and aesthetic view in setting the copper strips on the body.

  The third step is to apply the colour which is known as enamel filling. The colour or enamel is like the glaze on ceramics. It is called falang. Its basic elements are boric acid, saltpetre and alkaline. Due to the difference in the minerals added, the colour differs accordingly. Usually one with much iron will turn grey, with uranium, yellow, with chromium, green, with zinc, white, with bronze, blue, with gold or iodine, red. In time of filling, all the colours, ground beforehand into minute powder and contained in plates, are placed in front of the workers and are then applied to the little compartments separated by filigree.

  The fourth step is enamel firing. This is done by putting the article, with its enamel fillings, to the crucible. After a short moment, the copper body will turn red. But after firing, the enamel in the little compartment will sink down a bit. That will require a refilling. This process will go on repeatedly until the little compartments are finally filled.

  The fifth step is polishing. The first polish is with energy. Its aim is to make the filigree and the filled compartments even. The whole piece is again put to fire. Polish once more with a whet stone. Finally, use a piece of hard carbon to polish again so as to obtain some lustre on the surface of the article.

  The sixth step is gilding. This is done by placing the article in fluid of gold or silver. Add electric current. The exposed parts of the filigree and the metal fringes of the article will be smoothly and evenly gilded. After that, the metal part of the article will not get rusty. Then the article will again undergo another electroplating and a slight polish.

阅读:
录入:空气外

推荐 】 【 打印
相关新闻      
本文评论       全部评论
发表评论
  • 尊重网上道德,遵守中华人民共和国的各项有关法律法规
  • 承担一切因您的行为而直接或间接导致的民事或刑事法律责任
  • 本站管理人员有权保留或删除其管辖留言中的任意内容
  • 本站有权在网站内转载或引用您的评论
  • 参与本评论即表明您已经阅读并接受上述条款


点评: 字数
姓名:
精彩推荐
Google提供的广告